Oxidation Celadon · G2926B + 1.5 % iron · Cone 6 · 1 kg dry mix

$16.50
Green celadons are made by adding 1–2 % iron oxide to a clear base. This mix uses Digitalfire G2926B. Mix about 90 g water per 100 g powder to a specific gravity of 1.43–1.44 and sieve through 80 mesh; about 1 g Epsom salts per 1000 g powder makes it gel for even dipping. Fire with C6DHSC or PLC6DS.
Made with this
- Firing Curve Guide #1 | matte white glaze surface · Cone 6 · Oxidation
- Glaze Method Guide #7 | cup edge coverage · Cone 6 · Oxidation
- Firing Curve Guide #2 | cobalt blue glaze test · Cone 6 · Oxidation
- Glaze Effect Showcase #5 | slow-cool firing record · Cone 10 · Reduction
- Selected User Case #6 | vase glaze case · Cone 6 · Oxidation
- Glaze Method Guide #4 | clear glaze coverage test · Cone 018 · Oxidation
- Glaze Effect Showcase #6 | vase glaze case · Cone 04 · Oxidation
- Glaze Effect Showcase #3 | iron speckle texture · Cone 6 · Oxidation
- Selected User Case #1 | matte white glaze surface · Cone 018 · Oxidation